Effect Of Calcination Temperature On The Microstructure And Physical Properties Of Ba0.75−Xcaxla0.30fe12co0.25ti0.15o19 M-Type Barium Hexaferrites
DOI:
https://doi.org/10.5281/zenodo.24574728Keywords:
Barium Hexaferrite; Calcination Temperature; X-Ray Diffraction; Scherrer Equation; Sem; Vibrating Sample Magnetometer; Coercivity; Saturation MagnetizationAbstract
Ba0.75−x CaxLa0.30Fe12Co0.25Ti0.15O19 M-type barium hexaferrite powders were synthesized by the solid-state reaction route and the powders were heat treated for 12 hours at four progressively higher temperatures (1130, 1140, 1150, and 1160 °C) to trace the effect of thermal treatment on phase formation, crystallite growth, surface morphology and magnetic behavior within this system. The X-ray diffraction pattern at all the calcination temperatures revealed a high percentage of one hexagonal M-type magneto plumbite phase corresponding to JCPDS card No. 43-0002 and weak traces of another α-Fe2O3 phase indicating the incomplete crystallization at the lower temperature end. The principal reflections were used to derive the crystallite size using the Debye–Scherrer relation, which showed that as the calcination temperature increased, the crystallite size increased progressively from 41.72 nm at 1130 °C to 89.75 nm at 1160 °C, in line with the expected thermally induced grain growth. Scanning electron microscopy showed monodisperse, hexagonal nanoplates consistent with the magnetoplumbite structure, which become coarser and more agglomerated as the temperature rises. Vibrating sample magnetometry revealed that saturation magnetization remained nearly constant between 1130 °C and 1140 °C (around 63.30 emu/g), then decreased to 57.43 emu/g at 1150 °C and further to 49.99 emu/g at 1160 °C. Meanwhile, coercivity increased from 2024 Oe to 2451 Oe over this temperature range. These patterns suggest a competition between grain growth, cation redistribution among the tetrahedral, octahedral and bipyramidal sites in the hexaferrite lattice and the resulting changes in super exchange interaction strength and magneto crystalline anisotropy. Overall, the findings demonstrate that calcination temperature is an effective and simple means to tune the crystallite size, remanence and coercivity of La–Ca–Co–Ti substituted M-type barium hexaferrites, useful in permanent magnets and high-frequency applications.